TECATRON PPS CM XP64 black
modified PPS
This compression molded PPS material is modified with 40% glass fibers for increased strength and stiffness.
Mechanical properties | Value | Unit | Parameter | Norm |
---|---|---|---|---|
Tensile strength | 8,300 | psi | ASTM D 638 | |
Elongation at break (tensile test) | 1.3 | % | @73°F | ASTM D 638 |
Modulus of elasticity (tensile test) |
1,355,000 | psi | @73°F | ASTM D 638 |
Flexural strength | 14,000 | psi | ASTM D 790 | |
Modulus of elasticity (flexural test) |
1,230,000 | psi | @73°F | ASTM D 790 |
Compression strength | 20,000 | psi | @ 10% | ASTM D 695 |
Impact strength (Izod) | 0.45 | ftlbsin | notched | ASTM D 256 |
Shore hardness | 90 | D Scale | ASTM D 2240 | |
Compression strength | 7,800 | psi | @ 1% | ASTM D 695 |
Compression strength | 19,500 | psi | Max Load | ASTM D 695 |
Compression modulus | 700,000 | psi | @73°F | ASTM D 695 |
Electrical properties | Value | Unit | Parameter | Norm |
---|---|---|---|---|
Dielectric strength | 23.3 | kV/mm | ASTM D 149 | |
Dielectric constant | 4.58 | 500Hz, 200°C | ASTM D 150 | |
volume resistance | 2.91 | O*cm | ASTM D 257 |
Other properties | Value | Unit | Parameter | Norm |
---|---|---|---|---|
Moisture absorption | 0.03 | % | ASTM D 570 |