TECANYL® black (Noryl EN 265)

polyphenylene oxide

​TECANYL PPE black, (made with Noryl® EN265) due to its inherent chemical composition, exhibits unusually low moisture absorption. Therefore, good electrical insulating properties are realized over a wide range of humidity and temperature conditions. Chemical attack from water, most salt solutions, acids and bases is also minimal with TECANYL. The addition of glass fiber reinforcement enhances both the mechanical and thermal properties of the basic TECANYL material. Made from Sabic Noryl® EN265 resin.

Facts

Chemical designation
PPO (Polyphenylene oxide)
Color
black
Density
1,08 g/cm3

Main Features

  • electrically insulating
  • high strength
  • good dimensional stability
  • high toughness
  • high thermal resistance

Target industries

Technical details


  • Mechanical properties
    Mechanical propertiesValueUnitConditionTest Method
    Tensile strength at break9,200psi@ 73 °FASTM D 638
    Modulus of elasticity
    (tensile test)
    350,000psi@ 73 °FASTM D 638
    Elongation at break25%@ 73 °FASTM D 638
    Flexural strength13,400psi@ 73 °FASTM D 790
    Modulus of elasticity
    (flexural test)
    370,000psi@ 73 °FASTM D 790
    Impact strength (Izod)3.5ftlbsin@ 73 °FASTM D 256
    Rockwell hardness119-@ 73 °FASTM D 785
    Coefficient of friction0.32-StaticASTM D 3702
    Coefficient of friction0.39-Dynamic, 40 psi, 50 fpmASTM D 3702
    Tensile strength at yield9,000psi@ 73 °FASTM D 638
  • Thermal properties
    Thermal propertiesValueUnitConditionTest Method
    Deflection temperature279F@ 66 psiASTM D 648
    Deflection temperature254F@264 psiASTM D 648
    Thermal expansion (CLTE)3.3*10-5ininFASTM D 696
    Service temperature230FIntermittent-
    Service temperature220FLong Term-
    Vicat softening point310F-
  • Electrical properties
    Electrical propertiesValueUnitConditionTest Method
    Volume resistivity1*1017O*cm@ 73 °FASTM D 257
    Dielectric strength500V/milASTM D 149
    Dielectric constant2.7-@ 60 Hz, 73 °F, 50% RHASTM D 150
    Dissipation factor0.0007-@ 60 Hz, 73 °FASTM D 150
  • Other properties
    Other propertiesValueUnitConditionTest Method
    Moisture absorption0.07%@ 24 hrs, 73 °FASTM D 570
    Flammability (UL94)V1--
    Flammability (UL94)V0--

Stock program