TECAPEEK CM XP92 natural
PEEK compression molded, filled with. 15% glass fibre
This compression molded material is a Victrex® PEEK polymer modified with 15% glass fibre for increased strength.
>
Mechanical properties | Value | Unit | Parameter | Norm |
---|---|---|---|---|
Tensile strength | 103 | MPa | ASTM D 638 | |
Elongation at break (tensile test) | 3.8 | % | ASTM D 638 | |
Flexural strength | 149 | MPa | ASTM D 790 |
Thermal properties | Value | Unit | Parameter | Norm |
---|---|---|---|---|
Melting temperature | 342 | C | DSC | - |
Relative costs | Value | Unit | Parameter | Norm |
---|---|---|---|---|
Relative costs EU from € to €€€€€€ | €€€€€ |