TECATRON PPS CM XP64 natural
modified PPS
                        This compression molded PPS material is modified with 40% glass fibres for increased strength and stiffness.
                    
                    | Mechanical properties | Value | Unit | Parameter | Norm | 
|---|---|---|---|---|
| Modulus of elasticity  (tensile test)  | 
                                                            6200 | MPa | ASTM D 638 | |
| Tensile strength | 42 | MPa | ASTM D 638 | |
| Elongation at break (tensile test) | 1.1 | % | ASTM D 638 | |
| Flexural strength | 75 | MPa | ASTM D 790 | |
| Modulus of elasticity  (flexural test)  | 
                                                            8200 | MPa | ASTM D 790 | |
| Compression modulus | 3900 | MPa | ASTM D 695 | |
| Compression strength | 172 | MPa | ASTM D 695 | |
| Shore hardness | 88 | - | Shore D | ASTM D 2240 | 
| Thermal properties | Value | Unit | Parameter | Norm | 
|---|---|---|---|---|
| Heat distortion temperature | 112 | C | ASTM D 648 | 
| Relative costs | Value | Unit | Parameter | Norm | 
|---|---|---|---|---|
| Relative costs EU from € to €€€€€€ | €€€€ |